Fomapan 200@160 in NUCLEOL BF200 2%A+1,5%B

FILM

Foma Fomapan 200

FILM SIZE
120/220
EXPOSURE INDEX
160
DEVELOPER

NUCLEOL BF200

DILUTION
2%A+1,5%B
TEMPERATURE (° C)
25
AGITATION
Every 60 sec.
NOTES
Primo minuto agitazione continua, poi 4 inversioni ogni 60 sec 